Effect of equal-channel angular pressing on pitting corrosion resistance of anodized aluminum-copper alloy

  • In Joon SON
  • , Hiroaki NAKANO
  • , Satoshi OUE
  • , Shigeo KOBAYASHI
  • , Hisaaki FUKUSHIMA
  • , Zenji HORITA
  • Kyushu University
  • Kyushu Sangyo University

Research output: Contribution to journalArticlepeer-review

30 Scopus citations

Fingerprint

Dive into the research topics of 'Effect of equal-channel angular pressing on pitting corrosion resistance of anodized aluminum-copper alloy'. Together they form a unique fingerprint.
Sort by

Material Science