Effect of filament configuration on critical current density of Bi2212/Ag wires with low Ag ratio

  • Sang Cheol Kim
  • , Dong Woo Ha
  • , Sang Soo Oh
  • , Il Yong Han
  • , Jae Geun Oh
  • , Ho Sang Sohn

Research output: Contribution to journalArticlepeer-review

7 Scopus citations

Abstract

Effect of filament configuration and heat treatment of Bi2212/Ag round wire with low Ag ratio on the engineering critical current density (Je) was reported. We have fabricated 55 × 7, 85 × 7, and 121 × 7 wires with different Ag ratio and evaluated Je at various wire diameters. We have also changed the parameters of heat treatment. The effects of maximum process temperature (Tmax) and soaking time at T max and average filament diameter on the Je were also studied. 121 × 7 wire of 0.95 mm diameter heat-treated at Tmax = 888°C showed Je of 858 A/mm2 at 4.2 K, 0 T.

Original languageEnglish
Article number4519992
Pages (from-to)1188-1191
Number of pages4
JournalIEEE Transactions on Applied Superconductivity
Volume18
Issue number2
DOIs
StatePublished - Jun 2008

Keywords

  • Bi2212/Ag wire
  • Critical current density
  • Multi-filamentary wire
  • Powder-in-tube