Nonplanar Atomic Layer Deposition (ALD)-Niobium Oxide (NbOx) Neurons for Oscillatory Neural Network Applications

  • Jaehyun Moon
  • , Kitae Kim
  • , Jihyun Kim
  • , Soohyung Park
  • , Yeonjin Yi
  • , Jiyong Woo
  • , Seung Youl Kang
  • Electronics and Telecommunications Research Institute
  • University of Science and Technology UST
  • Yonsei University
  • Korea Institute of Science and Technology
  • Kyungpook National University

Research output: Contribution to journalArticlepeer-review

Abstract

This article presents a nonplanar niobium oxide (NbOx) neuron device fabricated using an atomic layer deposition (ALD) method for use in oscillatory neural networks (ONNs). Potentially, such nonplanar geometry allows for high-density arrays. The desired threshold switching (TS) characteristics are achieved through an interfacial method using a thin titanium (Ti) layer. X-ray photoelectron spectroscopy (XPS) analysis confirms that the oxyphilic Ti layer reduces Nb2O5 to the desired NbO2 stoichiometry, which is crucial for the device's functionality. The device demonstrates S-type negative differential resistance (NDR) under current-controlled operation, and its self-oscillation capabilities are verified within an electrical oscillator circuit. The oscillation frequency is shown to increase linearly with the applied voltage (Vd). The nonplanar structure and the use of a Ti layer to tune the material's properties allow for the realization of a compact, low-power neuromorphic device without the need for additional thermal annealing. Finally, the study demonstrates the practical application of these NbOx neurons in an ONN architecture for pattern recognition. The system successfully recognizes binary representations of digits. The network's functionality relies on phase synchronization between neurons, where a binary pattern is encoded by applying a delayed VDD to each neuron pixel.

Original languageEnglish
Article numbere202501015
JournalAdvanced Intelligent Systems
Volume8
Issue number4
DOIs
StatePublished - Apr 2026

Keywords

  • artificial neuron
  • atomic layer deposition
  • niobium oxide
  • oscillatory neural network
  • oxyphilic layer

Fingerprint

Dive into the research topics of 'Nonplanar Atomic Layer Deposition (ALD)-Niobium Oxide (NbOx) Neurons for Oscillatory Neural Network Applications'. Together they form a unique fingerprint.

Cite this